Material Designations
UNS N06617
W.Nr. 2.4663a
EN NiCr23Co12Mo
AFNOR NC22K12D9A
Chemical Composition Range
Nickel (Ni): 44.50 min (Balance ~52.00 - 55.00)
Chromium (Cr): 20.00 - 24.00
Cobalt (Co): 10.00 - 15.00
Molybdenum (Mo): 8.00 - 10.00
Aluminum (Al): 0.80 - 1.50
Carbon (C): 0.05 - 0.15
Iron (Fe): 3.00 max
Manganese (Mn): 1.00 max
Silicon (Si): 1.00 max
Titanium (Ti): 0.60 max
Copper (Cu): 0.50 max
Boron (B): 0.006 max
Sulfur (S): 0.015 max
Phosphorus (P): 0.015 max
Physical Properties
Density: 8.36 g/cm³ (0.302 lb/in³)
Melting Range: 1332°C - 1380°C (2430°F - 2510°F)
Specific Heat (26°C): 419 J/kg·K (0.100 Btu/lb·°F)
Electrical Resistivity (26°C): 1.22 µΩ·m (736 ohm·circ mil/ft)
Mechanical Properties (Typical, Solution Annealed)
Tensile Strength: 760 - 900 MPa (110 - 130 ksi)
Yield Strength (0.2% Offset): 310 - 450 MPa (45 - 65 ksi)
Elongation: 35% - 50%
Hardness: 80 - 95 HRB
Scrap and Foundry Classification
Primary Alloy Category: High Nickel-Chromium-Cobalt Superalloy Scrap
Scrap Forms: Solids, Turnings, Millings, Offcuts, Castings, Foundry Remelt Ingot/Billet
Key Impurity Limits for Foundry Remelt: Silicon <= 0.50%, Iron <= 1.50%, Sulfur <= 0.005%, Oil/Grease < 0.10%
Applicable Specifications
ASTM B166 (Rod, Bar, Wire)
ASTM B168 (Plate, Sheet, Strip)
ASTM B167 (Seamless Pipe and Tube)
ASTM B564 (Forgings)
SAE AMS 5887 (Bars, Forgings)
SAE AMS 5888 (Plate)
SAE AMS 5889 (Sheet, Strip)
AWS A5.14 ERNiCrCoMo-1 (Bare Wire)
AWS A5.11 ENiCrCoMo-1 (Covered Electrodes)
Price:
Thank You!
Thank You for your valuable time. We have received your details and will get back to you shortly.
For an immediate response, please call this
number 08045800544
Price:
English
Spanish
French
German
Italian
Chinese (Simplified)
Japanese
Korean
Arabic
Portuguese